Mostrar el registro sencillo del registro

dc.rights.licenceAtribución-NoComercial-SinDerivadas 4.0 Internacional*
dc.contributor.advisorGómez Méndez, Luis David
dc.contributor.advisorGutiérrez Rojas, Ivonne del Socorro
dc.contributor.authorHernández Gómez, María Paula
dc.date.accessioned2022-05-16T12:34:34Z
dc.date.available2022-05-16T12:34:34Z
dc.date.created2021-12-09
dc.identifier.urihttp://hdl.handle.net/10554/59776
dc.description.abstractEn los últimos años se ha incrementado el uso de plásticos debido a las mejoras del material para hacerlo altamente resistente a diferentes condiciones ambientales e incluso a la acción de los microorganismos. Lo anterior conduce a la difícil degradación de los plásticos ordinarios y como consecuencia una alta preocupación ambiental mundial frente al impacto negativo de estos desechos. Particularmente, uno de los elementos hecho de polímeros sintéticos, como el polipropileno (PP) y polietileno (PE) son los pitillos plásticos, dichos utensilios son desechados sin a travesar un proceso adecuado de reciclaje o reúso, por lo que a cambio el mercado rápidamente comenzó a ofrecer alternativas como los pitillos plásticos oxo-biodegradables que contienen pro-oxidantes en su composición, lo que lleva a establecer técnicas físico químicas como la degradación con luz UV y el estudio de microorganismos potencialmente degradadores de plástico, como es el caso de Phanerochaete sp, hongo de podredumbre blanca que cuenta con enzimas como la manganeso peroxidasa y la lignino peroxidasa. Es por esta razón que este estudio plantea como objetivo evaluar la degradación de pitillos oxobiodegradables (OB) pretratados con luz ultravioleta (UV) en un sistema de microcosmos inoculado con Phanerochaete sp. Para cumplir con lo mencionado se tomaron fragmentos de pitillos oxo-biodegradables que fueron expuestos por 300 horas a luz UV y posteriormente expuestos por 72 días, en sistema de microcosmos, para llevar a cabo un tratamiento biológico con Phanerochaete sp. La degradación fue medida empleando la técnica FTIR, AFM y técnica de ángulo de contacto, adicionalmente se realizó la caracterización de otros microorganismos que se encontraban en el sistema. Se determinó que el pretratamiento planteado de fotólisis no genero cambios importantes en la superficie de los fragmentos de pitillo oxo-biodegradable, se evidenció la colonización de micelio fúngico y la transformación particular de los fragmentos de pitillo oxo-biodegradables en la réplica TR4 que contó con la presencia de Serratia ficaria, Phanerochaete sp, Talaromyces sp, y en menor medida de Rhodotorula mucilaginosa y Geotrichum sp , evidenciándose una diminución del ángulo de contacto de (65± 5) % respecto al fragmento de plástico prístino, además de la oxidación del material detectado por movimientos de tensión O-H a (3300 ± 10) cm-1 y enlaces C-OH a (1260 ± 10) cm-1 y a (670± 10) cm-1 a demás de movimientos de tensión C=O (1625 ± 10) cm-1. A partir de lo anterior se concluye que pretratamiento planteado de fotólisis no aporto a la degradación del material como se esperaba, sin embargo estos cambios del TR4 son atribuidos a un efecto sinérgico entre los microorganismos presentes en la réplica TR4.spa
dc.formatPDFspa
dc.format.mimetypeapplication/pdfspa
dc.language.isospaspa
dc.publisherPontificia Universidad Javerianaspa
dc.rights.urihttp://creativecommons.org/licenses/by-nc-nd/4.0/*
dc.subjectPlásticospa
dc.subjectOxo-biodegradablespa
dc.subjectDegradaciónspa
dc.subjectPhanerochaete spspa
dc.titleEvaluación de la degradación de pitillos oxo-biodegradables previamente tratados con fotólisis en un sistema de microcosmos, inoculado con Phanerochaete sp CMPUJH123spa
dc.type.hasversionhttp://purl.org/coar/version/c_ab4af688f83e57aa
dc.title.englishEvaluation of the degradation of oxo-biodegradable straws previously treated with photolysis in a microcosm system inoculated with Phanerochaete sp CMPUJH123spa
dc.subject.keywordPlasticspa
dc.subject.keywordDegradationspa
dc.subject.keywordOxo-biodegradablespa
dc.subject.keywordPhanerochaete spspa
dc.description.abstractenglishDuring the last years, the use of plastics has increased due to improvements in the material to make it highly resistant to different environmental conditions and even to the action of microorganisms. This leads to the difficult degradation of ordinary plastics and as a consequence a high environmental concern worldwide about the negative impact of these wastes. Particularly, one of the elements made of synthetic polymers, such as polypropylene (PP) and polyethylene (PE) are plastic straws, such utensils are discarded without going through a proper recycling or reuse process, so in return, the market quickly began to offer alternatives such as oxo-biodegradable plastic straws containing pro-oxidants in its composition, This led to the establishment of physical-chemical techniques such as degradation with UV light and the study of microorganisms potentially degrading plastic, as is the case of Phanerochaete sp, a white-rot fungus that has enzymes such as manganese peroxidase and lignin peroxidase. For this reason, this study evaluated the degradation of oxo-biodegradable (OB) straws pretreated with ultraviolet (UV) light in a microcosm system inoculated with Phanerochaete sp. To comply with the above, fragments of oxo-biodegradable straws were exposed for 300 hours to UV light and then exposed for 72 days, in a microcosm system, to carry out a biological treatment with Phanerochaete sp. The degradation was measured using the FTIR technique, AFM, and contact angle technique; additionally, the characterization of other microorganisms that were in the system was carried out. It was determined that the proposed photolysis pretreatment did not generate important changes on the surface of the oxo-biodegradable straw fragments, the colonization of fungal mycelium, and the particular transformation of the oxo-biodegradable straw fragments was evidenced in the TR4 replicate, which had the presence of Serratia ficaria, Phanerochaete sp, Talaromyces sp, and to a lesser extent Rhodotorula mucilaginosa and Geotrichum sp, evidencing a decrease in the contact angle of (65± 5) % concerning the pristine plastic fragment, in addition to the oxidation of the material detected by O-H tension movements at (3300 ± 10) cm-1 and C-OH bonds at (1260 ± 10) cm-1 and at (670± 10) cm-1 in addition to C=O tension movements (1625 ± 10) cm-1. Finally, it was concluded that the photolysis pretreatment did not contribute to the degradation of the material as expected; however, these changes in TR4 were attributed to a synergistic effect among the microorganisms present in the TR4 replicate.spa
dc.rights.accessrightsinfo:eu-repo/semantics/openAccess
dc.publisher.programMicrobiología Industrialspa
dc.publisher.facultyFacultad de Cienciasspa
dc.type.localTesis/Trabajo de grado - Monografía - Pregradospa
dc.subject.armarcMicrobiología industrial - Tesis y disertaciones académicasspa
dc.subject.armarcFotoquímicaspa
dc.subject.armarcBiodegradaciónspa
dc.subject.armarcPlásticosspa
dc.description.degreenameMicrobiólogo (a) Industrialspa
dc.description.degreelevelPregradospa
dc.identifier.instnameinstname:Pontificia Universidad Javerianaspa
dc.identifier.reponamereponame:Repositorio Institucional - Pontificia Universidad Javerianaspa
dc.identifier.repourlrepourl:https://repository.javeriana.edu.cospa
dc.type.coarhttp://purl.org/coar/resource_type/c_7a1f
dc.rights.localDe acuerdo con la naturaleza del uso concedido, la presente licencia parcial se otorga a título gratuito por el máximo tiempo legal colombiano, con el propósito de que en dicho lapso mi (nuestra) obra sea explotada en las condiciones aquí estipuladas y para los fines indicados, respetando siempre la titularidad de los derechos patrimoniales y morales correspondientes, de acuerdo con los usos honrados, de manera proporcional y justificada a la finalidad perseguida, sin ánimo de lucro ni de comercialización. De manera complementaria, garantizo (garantizamos) en mi (nuestra) calidad de estudiante (s) y por ende autor (es) exclusivo (s), que la Tesis o Trabajo de Grado en cuestión, es producto de mi (nuestra) plena autoría, de mi (nuestro) esfuerzo personal intelectual, como consecuencia de mi (nuestra) creación original particular y, por tanto, soy (somos) el (los) único (s) titular (es) de la misma. Además, aseguro (aseguramos) que no contiene citas, ni transcripciones de otras obras protegidas, por fuera de los límites autorizados por la ley, según los usos honrados, y en proporción a los fines previstos; ni tampoco contempla declaraciones difamatorias contra terceros; respetando el derecho a la imagen, intimidad, buen nombre y demás derechos constitucionales. Adicionalmente, manifiesto (manifestamos) que no se incluyeron expresiones contrarias al orden público ni a las buenas costumbres. En consecuencia, la responsabilidad directa en la elaboración, presentación, investigación y, en general, contenidos de la Tesis o Trabajo de Grado es de mí (nuestro) competencia exclusiva, eximiendo de toda responsabilidad a la Pontifica Universidad Javeriana por tales aspectos. Sin perjuicio de los usos y atribuciones otorgadas en virtud de este documento, continuaré (continuaremos) conservando los correspondientes derechos patrimoniales sin modificación o restricción alguna, puesto que, de acuerdo con la legislación colombiana aplicable, el presente es un acuerdo jurídico que en ningún caso conlleva la enajenación de los derechos patrimoniales derivados del régimen del Derecho de Autor. De conformidad con lo establecido en el artículo 30 de la Ley 23 de 1982 y el artículo 11 de la Decisión Andina 351 de 1993, "Los derechos morales sobre el trabajo son propiedad de los autores", los cuales son irrenunciables, imprescriptibles, inembargables e inalienables. En consecuencia, la Pontificia Universidad Javeriana está en la obligación de RESPETARLOS Y HACERLOS RESPETAR, para lo cual tomará las medidas correspondientes para garantizar su observancia.spa
dc.rights.coarhttp://purl.org/coar/access_right/c_abf2spa


Ficheros en el registro

Thumbnail
Thumbnail

Este registro aparece en la(s) siguiente(s) colección(ones)

Mostrar el registro sencillo del registro

Atribución-NoComercial-SinDerivadas 4.0 Internacional
Excepto si se señala otra cosa, la licencia del registro se describe como Atribución-NoComercial-SinDerivadas 4.0 Internacional